Estándares AA Grado 5083 O
Propiedades
Generales
Propiedad | Valor | Condición | Estándares relacionados |
---|---|---|---|
Densidad | 2,66 g/cm³ | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Mecánica
Propiedad | Valor | Condición | Estándares relacionados | Comentario |
---|---|---|---|---|
Módulo elástico | 71,0 GPa | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 | |
Tenacidad a la fractura por deformación plana | 22,0 - 35,0 MPa·√m | Típico para aluminio forjado serie 5000 | ||
Relación de Poisson | 0.33 [-] | Típico para aluminio forjado serie 5000 | ||
Módulo de corte | 26,0 - 26,5 GPa | Típico para aluminio forjado serie 5000 | ||
Resistencia a la tracción | 250,0 MPa | O | Normas AA, ASTM B209 | |
255,0 MPa | O | Normas AA, ASTM B209 | ||
260,0 MPa | O | Normas AA, ASTM B209 | ||
270,0 - 345,0 MPa | O | Normas AA, ASTM B209, ASTM B547 | ||
270,0 - 350,0 MPa | O | Normas AA, ASTM B210, ASTM B221, ASTM B241, ASTM B345 | ||
275,0 - 350,0 MPa | O | Normas AA, ASTM B209, ASTM B547 | ||
290,0 MPa | O | Normas AA |
térmica
Propiedad | Temperatura | Valor | Condición | Estándares relacionados | Comentario |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 20 °C | 2.38e-05 1/K | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 | |
100 °C | 2.38e-05 1/K | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 | ||
Temperatura máxima de servicio | 150,0 °C | Típico para aluminio forjado serie 5000 | |||
Punto de fusión | 580,0 - 640,0 °C | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 | ||
Capacidad calorífica específica | 879,0 - 963,0 J/(kg·K) | Típico para aluminio forjado serie 5000 | |||
Conductividad térmica | 117.0 | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Eléctrico
Propiedad | Valor | Condición | Estándares relacionados |
---|---|---|---|
Conductividad eléctrica | 17000000.0 S/m | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Resistividad eléctrica | 5,88e-08 Ω·m | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Propiedades químicas
Propiedad | Valor | Condición | Estándares relacionados |
---|---|---|---|
Cromo | 0,05 - 0,25 % | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Cobre | 0,1 % | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Hierro | 0,40 % | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Magnesio | 4,0 - 4,9 % | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Manganeso | 0,4 - 1,0 % | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Silicio | 0,4 % | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Titanio | 0,15 % | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Cinc | 0,25 % | O | Normas AA, ASTM B209, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B547 |
Propiedades tecnológicas
Propiedad | ||
---|---|---|
Brazing | general:no se conoce ni se desarrolla ninguna soldadura fuerte
| |
Propiedades de corrosión | Agrietamiento por corrosión bajo tensión:kein Schadensfall im Betrieb und bei Labortests (O, H321, H116), kein Schadensfall im Betrieb, eingeschränkte Schäden bei den Labortests (H111), general:muy bueno, sin protección en atmósfera industrial o de agua de mar
| |
Mecanizabilidad general | General:pobre
| |
Trabajabilidad | general (estado):aceptable (O), deficiente (H321, H116, H111)
|
Metal
- Estándares de grado AA 5083 H321
- Estándares AA Grado 5456 O
- Estándares AA Grado 5083 H116
- Estándares AA Grado 6066 T6
- Estándares AA Grado 6351 T6
- Estándares AA Grado 5454 O
- Estándares AA Grado 1060 O
- Estándares AA Grado 3004 O
- Estándares de grado AA 5083 H32
- Estándares AA Grado 5050 O
- Estándares AA Grado 5154 O